Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.450 GPa @Temperature 23.0 °C |
65.3 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Flexural Modulus | 0.450 GPa @Temperature 23.0 °C |
65.3 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Flexural Modulus | 0.450 GPa @Temperature 120 °C |
65.3 ksi @Temperature 248 °F |
ASTM D790 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 0.450 GPa | 65.3 ksi | ISO 178 |
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Flexural Modulus | 0.450 GPa | 65.3 ksi | ASTM-D790 |
Polyram PlusTek RD101 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 0.450 GPa | 65.3 ksi | ASTM-D790 |
Polyram PlusTek PD100 Nylon 12, Injection Molding Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 0.450 GPa | 65.3 ksi | SAE J949 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.450 - 1.40 GPa @Temperature 60.0 - 120 °C |
65.3 - 203 ksi @Temperature 140 - 248 °F |
Average value: 0.883 GPa Grade Count:1 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |