Mechanical Properties Metric English Comments
Flexural Modulus 0.500 GPa
72.5 ksi
ISO 178
Polimeri Europa Flexirene® MR 50 A Linear Low Density Polyethylene
Flexirene MR 50 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity...
Flexural Modulus 0.500 GPa
72.5 ksi
ISO 178
Polimeri Europa Flexirene® MR 50 U Linear Low Density Polyethylene
Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 U are characterized by optimum rigidity...
Flexural Modulus 0.500 GPa
72.5 ksi
ISO 178
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene
Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity...
Flexural Modulus 0.500 GPa

@Temperature 90.0 °C
72.5 ksi

@Temperature 194 °F
ISO 178, ASTM D790
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
Flexural Modulus >= 0.500 GPa
>= 72.5 ksi
ASTM D1238
NIZHNEKAMSKNEFTEKHIM PE 4025W (25425) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus 0.500 - 0.500 GPa

@Temperature 90.0 - 90.0 °C
72.5 - 72.5 ksi

@Temperature 194 - 194 °F
Average value: 0.500 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
NOVA Chemicals Sclair® 96A HDPE Extrusion Resin  (discontinued **)
Features: Excellent processability, excellent stretchability, superior strength, gel free.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial oriented films.Data provide..
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
NOVA Chemicals Sclair® 96A-UV8D HDPE Extrusion Resin  (discontinued **)
Features: Excellent processability, excellent stretchability, superior strength, gel free, excellent UV resistance.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial or..
Flexural Modulus 0.500 GPa

@Temperature 120 °C
72.5 ksi

@Temperature 248 °F
ASTM D790
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Reliance Industries Reclair ER-19
Reclair ER-19 is a Octene Conomer based medium density Polyethylene grade designed for Rotational Molding applications with optimum loading of UV Stabilizer. Processing is similar to Butene grades...
Flexural Modulus 0.500 GPa

@Temperature 65.0 °C
72.5 ksi

@Temperature 149 °F
ASTM D790
BASF Capron® 8200 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.500 GPa

@Temperature 65.0 °C
72.5 ksi

@Temperature 149 °F
ASTM D790
BASF Capron® 8202 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE.
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Covestro Bayflex® 110 RIM-LITE Polyurethane Elastomeric RIM, 13% Mineral Filled, MDI-based 2-Component Liquid System
Contains 10% calcium silicate and 3% glass microspheres.0.15 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, ..
Flexural Modulus 0.500 GPa
72.5 ksi
ISO 178
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Flexural Modulus 0.500 GPa
72.5 ksi
After conditioning at 23°C and 50% RH; ISO 178
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Flexural Modulus 0.500 GPa
72.5 ksi
Dry; ISO 178
Arkema Group Orgalloy® LT 4060 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Flexural Modulus 0.500 GPa
72.5 ksi
Dry; ISO 178
Arkema Group Orgalloy® LT 4060 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Flexural Modulus 0.500 GPa
72.5 ksi
SAE J949
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Buckeye Polymers BP Flex A9505 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
Flexural Modulus 0.500 GPa

@Temperature 65.0 °C
72.5 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Flexural Modulus 0.500 GPa

@Temperature 65.0 °C
72.5 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
Flexural Modulus 0.500 GPa
72.5 ksi
After conditioning at 23°C and 50% RH; ISO 178
Arkema Group Orgalloy® LT 5050 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Buckeye Polymers BP Flex D0853 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
Flexural Modulus 0.500 - 4.83 GPa
72.5 - 700 ksi
Average value: 1.19 GPa Grade Count:63
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Buckeye Polymers BP Flex D4507 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
Flexural Modulus 0.500 GPa

@Temperature 23.0 °C
72.5 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET  (Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont
Flexural Modulus 0.500 GPa
72.5 ksi
After conditioning at 23°C and 50% RH; ISO 178
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Copyright © lookpolymers.com All Rights Reserved