Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D790 |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D790 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D790 |
ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene providing an excellent processing window for molding toys and consumer items. The resin is formulated to provi.. |
|||
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D747 |
Ineos K44-11-128 HDPE Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi.. |
|||
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D790 |
Ecomass® 4703ZC87 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D790 |
PolyOne Stat-Tech™ UR-7SS-5GF/000 PT GY Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Stainless Steel Fiber FilledGlass Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 0.579 GPa | 84.0 ksi | ASTM D790 |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |