Material Notes:
Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. This material combines excellent processability and environmental stress crack resistance (ESCR) with well-balanced end use properties. This resin meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D4883
High Load Melt Index 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 23.8 MPa
3450 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 850 %
850 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 0.579 GPa
84.0 ksi
ASTM D747
0.841 GPa
122 ksi
2% Secant-Method 1; ASTM D790
Izod Impact, Notched 4.70 J/cm
8.81 ft-lb/in
Partial break; ASTM D256
Tensile Impact Strength 710 kJ/m²
338 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Region US & Canada
Bamberger Polymers Distribution