Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.952 GPa | 138 ksi | UNI EN ISO 14125: 2000 |
CRP Technology Windform® FX Polyamide Composite Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive.. |
|||
Flexural Modulus | 0.952 GPa | 138 ksi | |
Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |
|||
Flexural Modulus | 0.952 GPa | 138 ksi | |
Dow HDPE 38152M High Density Polyethylene DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent proces.. |