Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.950 GPa | 138 ksi | |
Plastcom SLOVALEN PQ 81 T 10 PP, 10% mineral filling FeaturesModified PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | |
Plastcom SLOVALEN PQ 91T 5 PP, 5% mineral filling FeaturesModified PP for injection moulding with the content of 5 % mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-2002 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.950 GPa @Temperature 23.0 °C |
138 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYten HDPE S801 HDPE, Good Abrasion Resistance, Excellent Sliding Properties Information provided by Polykemi AB |
|||
Flexural Modulus | >= 0.950 GPa | >= 138 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4240G (EP2S29B) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 0.950 - 3.05 GPa | 138 - 442 ksi | Average value: 1.81 GPa Grade Count:28 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Flexural Modulus | >= 0.950 GPa | >= 138 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4340S (EP2H49G) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Rotational Molded; ASTM D790 |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Iran Petrochemical (PCC) Moplen EP-T30 U Polypropylene Moplen EP-T30 U is a heterophasic copolymer for injection moulding applications. Moplen EP-T30 U combines outstanding processability with extremely high impact Resistance. Moplen EP-T 30 U is desig.. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Flexural Modulus | 0.953 GPa | 138 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB 68 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.953 GPa | 138 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com.. |
|||
Flexural Modulus | 0.953 GPa | 138 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | cond; ISO 178 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | Secant; ISO 178 |
ExxonMobil Exxtral™ BNT 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.Availability: Africa & Middle East, Asia Pacific, E.. |
|||
Flexural Modulus | 0.952 GPa | 138 ksi | |
Dow HDPE 25455N High Density Polyethylene DOW HDPE 25455N resin is a narrow molecular weight distribution copolymer designed to offer good stress crack resistance and gloss with excellent toughness. This resin has good processability over a.. |
|||
Flexural Modulus | 0.952 GPa | 138 ksi | |
Dow HDPE 38152M High Density Polyethylene DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent proces.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | SAE J949 |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Breplast Bretene PP Polypropylene Composite Recovered polypropylene compositeInformation provided by Breplast S.p.A. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Flexural Modulus | 0.950 GPa @Temperature 23.0 °C |
138 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |