Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.276 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos J50-200-178 HDPE
A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m..
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos T50-200 HDPE
Ineos T50-200 is a high density polyethylene copolymer of narrow molecular weight distribution. It is intended for injection molding applications which require high impact resistance and good envir..
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos T50-2000 HDPE
Ineos T50-2000 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It is c..
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos T50-3600 HDPE
Ineos T50-3600 is a high density polyethylene copolymer of narrow molecular weight distribution used primarily for high speed injection molding of thin-walled articles. It is characterized by a hig..
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos T50-500 HDPE
Ineos T50-500 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and en..
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos T50-800 HDPE
T50-800 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use ..
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Ineos J50-2000-119 HDPE
HDPE J50-2000-119 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It i..