Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos J50-200-178 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m.. |
|||
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-200 HDPE Ineos T50-200 is a high density polyethylene copolymer of narrow molecular weight distribution. It is intended for injection molding applications which require high impact resistance and good envir.. |
|||
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-2000 HDPE Ineos T50-2000 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It is c.. |
|||
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-3600 HDPE Ineos T50-3600 is a high density polyethylene copolymer of narrow molecular weight distribution used primarily for high speed injection molding of thin-walled articles. It is characterized by a hig.. |
|||
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-500 HDPE Ineos T50-500 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and en.. |
|||
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos T50-800 HDPE T50-800 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use .. |
|||
Flexural Modulus | 1.276 GPa | 185.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos J50-2000-119 HDPE HDPE J50-2000-119 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It i.. |