Material Notes:
Ineos T50-2000 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It is characterized by a high melt index which allows easy processing of medium to thin-walled articles. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D4883
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.276 GPa
185.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding
Region US & Canada
Bamberger Polymers Distribution