Flexural Modulus >= 1.586 GPa
>= 230.0 ksi
Secant 1%; ASTM D-790-95
Multibase Multi-Flex® TPO D 5308-20 BLK
Glass reinforced TOP with improved stiffness and retention of low temperature resistance.Data provided by Multibase.
Flexural Modulus 1.586 GPa
230.1 ksi
ASTM D790
Lucent Polymers CPP-220 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp
Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,..
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Modulus 1.586 GPa
230.0 ksi
tangent; ASTM D790
Entec Hypro™ PPC-CC20 Natural Copolymer Polypropylene, 20% Calcium Carbonate Filled
Information provided by Entec
Flexural Modulus 1.586 GPa
230.0 ksi
tangent; ASTM D790
Entec Hypro™ PPH-CC10 Natural Homopolymer Polypropylene, 10% Calcium Carbonate Filled
Information provided by Entec
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Modulus 1.586 GPa
230.0 ksi
ASTM D790
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..