Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 1.586 GPa | >= 230.0 ksi | Secant 1%; ASTM D-790-95 |
Multibase Multi-Flex® TPO D 5308-20 BLK Glass reinforced TOP with improved stiffness and retention of low temperature resistance.Data provided by Multibase. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | tangent; ASTM D790 |
Entec Hypro™ PPC-CC20 Natural Copolymer Polypropylene, 20% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-CC10 Natural Homopolymer Polypropylene, 10% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.586 GPa | 230.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |