Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.793 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.793 GPa
260.1 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 5014 CU W Calcium Carbonate Filled Polypropylene
Multi-Pro 5014 CU W is a calcium carbonate reinforced PP concentrate with balanced impact and stiffness properties. This product is specially formulated for lawn furniture, suitable for outdoor exp..
Flexural Modulus 1.793 GPa
260.1 ksi
ASTM D790
Ineos Nova 5810 High Impact Polystyrene  (discontinued **)
Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection ..
Flexural Modulus 1.793 GPa
260.1 ksi
ASTM D790
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Modulus 1.793 GPa
260.1 ksi
ASTM D790
Ineos Nova 5511 High Impact Polystyrene
Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C..
Flexural Modulus 1.793 GPa
260.1 ksi
Secant @ 1% strain; ASTM D790
Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated
A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release pro..
Flexural Modulus 1.793 GPa
260.1 ksi
ASTM D790
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Flexural Modulus 1.793 GPa
260.1 ksi
tangent; ASTM D790
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled
Information provided by Entec
Flexural Modulus 1.793 GPa
260.1 ksi
ASTM D790
Ineos Nova 5420 High Impact Polystyrene  (discontinued **)
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m..