Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.85 GPa | 268 ksi | ISO METHOD 178 |
NYCOA 2001 PA 6 high melt strength general extrusion and molding grade of nylon 6Information provided by NYCOA, Inc. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | |
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Nilit RECONYL B S20 Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, impact modified (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1111R Polypropylene Homopolymer CHARACTERISTICS: EXCELLENT HIGH STIFFNESS, HEAT STABILITY, HIGH FLOW CONTAIN LONG TERM HEAT AGING ADDITIVE APPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, COFFEE MAKER, HAIR DRYER |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | 3 points and 2 mm/min; ISO 178 |
Styron INSPIREâ„¢ TF1500 ESU Polypropylene Talc filled, high impact PP compound. INSPIREâ„¢ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization.Information provided.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Lubrizol Telene 1650 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB135HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | At 2 mm/min; ISO 178 |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178-93 |
Wellman Wellamid® XT1627-BK2 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Total PSI 7240 High Impact Polystyrene 7240 is a very high impact polystyrene for the extrusion industry. This grade has been designed to be diluted with crystal polystyrene (such as LACQRENE® 140, 1340 or 1540) at higher levels than c.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Eastman DuraStar DS1000 Polymer, Natural Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Eastman DURASTAR DS1010 Natural PCTA Copolyester DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to .. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Eastman DuraStar MN610 Polymer, Natural Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very .. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | 15mm/min; ASTM D790 |
Denka MALECCA K-700 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 1.85 GPa | 268 ksi | ISO 178 |
A.D. Compound Adene NCJA Homopolymer 30% CaCO3 Filled Polypropylene Information provided by A.D. Compound |