Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.51 GPa | 1524 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 10.51 GPa | 1525 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.51 GPa | 1525 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.51 GPa | 1525 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.51 GPa | 1525 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.51 GPa | 1525 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.51 GPa | 1525 ksi | ASTM D790 |
A. Schulman ComAlloy® E-13086 Glass/TFE Reinforced PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.51 GPa | 1524 ksi | ASTM D790 |
Plenco 50240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |