Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.379 - 0.7198 GPa | 55.0 - 104.4 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D0850 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |