Mechanical Properties Metric English Comments
Flexural Modulus 74.5 GPa
10800 ksi
Prepreg, Warp Direction, RT, Dry; ASTM D7264
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric
RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg. Straightforward 350°F Cure Designed for the unique requirements of satellite and missile structuresLow shrinka..
Flexural Modulus 74.5 GPa

@Temperature 25.0 °C
10800 ksi

@Temperature 77.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber
Information provided by HexCel