Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 74.5 GPa | 10800 ksi | Prepreg, Warp Direction, RT, Dry; ASTM D7264 |
Renegade Materials Corporation RM-5001 Cyanate Ester Prepreg, 3K 8HS Fabric RM-5001 cyanate ester is a very low outgassing, toughened, high performance prepreg. Straightforward 350°F Cure Designed for the unique requirements of satellite and missile structuresLow shrinka.. |
|||
Flexural Modulus | 74.5 GPa @Temperature 25.0 °C |
10800 ksi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |