Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.759 GPa | 110 ksi | ISO METHOD 178 |
NYCOA 2046 Copolymer Nylon 6/69 extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L63935 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering .. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
BASF Capron® 8224 HSL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.759 GPa | 110 ksi | ASTM D790 |
Flint Hills P5M5R-083 Random Copolymer Polypropylene Features: Radiation resistant. Product does not contain animal derived components. Phthalate-freeApplications: Injection molded parts. Radiation sterilizable medical devices and lab wareInforma.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.759 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM Test |
BASF Ultramid® 8270 HS PA6 (Conditioned) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin
(discontinued **) Features: Good impact strength, easy processability, high ESCR.Applications: Small part blow molding, high ESCR HIC applications.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D3350 |
Formosa Plastics Formolene® HP4306 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for l.. |
|||
Flexural Modulus | 0.759 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D3350 |
Formosa Plastics Formolene® HP4000 Pipe HDPE High Density Hexene Copolymer Formolene® HP4000 is a high performance copolymer that is designed for the most demanding requirements of non pressure pipe applications. It has good long-term hoop st.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Flam™ 1502 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |