Multibase Multi-Flam™ 1502 PP Black Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Flam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flam™ 1502 PP Black Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Density 0.987 g/cc
0.0357 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 - 0.013 cm/cm
0.010 - 0.013 in/in
ASTM D955
Melt Flow 2.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Strength 19.3 MPa
2800 psi
ASTM D790
Flexural Modulus 0.758 GPa
110 ksi
Method I (3 point load), Procedure B); ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Gardner Impact 23.73 J
17.50 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2