Polymer Property : Flexural Modulus = 12.2 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 12.2 GPa
1770 ksi
STN EN ISO 178
Plastcom SLOVAMID 6 GF 45 Polyamide 6, 45% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
PolyOne Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber  (discontinued **)
Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur..
Flexural Modulus 12.2 GPa
1770 ksi
(50.8 mm Span) 1mm/min; ASTM D790
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement  (discontinued **)
ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is ..
Flexural Modulus 12.2 GPa
1770 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
Flexural Modulus 12.2 GPa
1770 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
Flexural Modulus 12.2 GPa
1770 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific)
DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI (Asia Pacific)
LNP* THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0069S PA 66
LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
E-Polymers SEPAZ® V330FR 30% Glass Fiber Reinforced Flame Retardant PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..