Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP)

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP)
Manufacturer PolyOne Corporation
Trade Name Stat-Tech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber for low to high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 93.8 MPa
13600 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 15.8 GPa
2290 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 12.2 GPa
1770 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.506 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C

@Thickness 6.35 mm
500 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C

@Thickness 6.35 mm
403 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Static Decay 0.0020 sec
0.0020 sec
(Mil-B-81705C), 12% RH, 500 kV to 50 kV
Shielding Effectiveness 30 - 80 dB

@Frequency 2.00e+7 - 1.80e+10 Hz
30 - 80 dB

@Frequency 2.00e+7 - 1.80e+10 Hz
1/8 thickness
Processing Properties Metric English Comments
Melt Temperature 299 - 316 °C
570 - 601 °F
Descriptive Properties Value Comments
Features Antistatic
Conductive
Electrically Conductive
Electromagnetic Shielding (EMI)
Radio Frequency Shielding (RFI)
Statically Conductive
Filler / Reinforcement Carbon Fiber Reinforcement, 20% Filler by Weight
Forms Pellets
Generic Material LCP
Generic Name Liquid Crystal Polymer (LCP)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
RoHS Compliance RoHS Compliant
Uses Aerospace Applications
Automotive Electronics
Business Equipment
Computer Components
Connectors
Electrical Housing
Electrical/Electronic Applications
Housings
Copyright © lookpolymers.com All Rights Reserved