Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 40% Glass Fiber Reinforced , Nylon 66
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nylene® 9633 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 159 MPa
23000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 235 °C
455 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648