Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 15.9 GPa @Temperature 23.0 °C |
2310 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES Electrafil® J-1200/CF/40 NAT ABS |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ISO 178 |
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface .. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PA6/12 CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 50% Filler by WeightAppearance: Black and Natural ColorTPCI# 9814104Information provided by TP Composites, .. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S.. |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 15.9 GPa | 2300 ksi | ASTM D790 |
PolyOne Edgetek® NL-30CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.9 GPa | 2310 ksi | ASTM D790 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |