Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 1.103 GPa | >= 160.0 ksi | Secant 1%; ASTM D-790-95 |
Multibase Multi-Flex® TPO D-6606 BLK Data provided by Multibase. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-140 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-144 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | Tangent; ASTM D 790 |
Ineos B50-35H-011 HDPE Ineos B50-35H-011 is a high density polyethylene copolymer developed for blow molding applications. It is recommended for use in applications which require a combination of high top load strength a.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | Tangent-Method 1; ASTM D790 |
Ineos B50-35H-176 HDPE B50-35H is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmental s.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | Secant @ 1% strain; ASTM D790 |
Ineos H20A-00 Polypropylene Homopolymer A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic ag.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.103 GPa | 160.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |