Material Notes:
A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic agent. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.5 MPa
3700 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 30.3 MPa
4390 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 500 %
500 %
2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 15 %
15 %
2 in/min.; ASTM D638
Flexural Modulus 1.103 GPa
160.0 ksi
Secant @ 1% strain; ASTM D790
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256
Impact Test 9.00 J
6.64 ft-lb
TUP Impact; 1" radius tip on 1/16" plaque
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution