Polymer Property : Flexural Modulus = 2.137 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.137 GPa
309.9 ksi
ASTM D790-04
Objet FullCure® 830 Vero White Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping
Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Mo..
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping
Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero..
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping
Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero..
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
Ineos Nova 5730 High flow, High impact  (discontinued **)
High flow, High impact, USP Class VIApplications: Toys, Medical, HousewaresProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provi..
Flexural Modulus 2.137 GPa
309.9 ksi
ASTM D790
Stratasys® Polycarbonate
A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts ..
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 2.137 GPa
309.9 ksi
tangent; ASTM D790
Entec Hypro™ PPC-T30 Copolymer Polypropylene, 30% Talc Reinforced
Information provided by Entec
Flexural Modulus 2.137 GPa
310.0 ksi
XY direction; ASTM D790
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech..
Flexural Modulus 2.137 GPa
310.0 ksi
ASTM D790
Ineos Nova 5711 High Impact Polystyrene  (discontinued **)
High flow, High impact, USP Class VIApplications: Thin wall, Medical, Housewares, ToysProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Inform..
Flexural Modulus 2.137 GPa
309.9 ksi
ASTM D790-04
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..