Mechanical Properties Metric English Comments
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
PolyOne Geon™ Vinyl Packaging VE0-112 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.66 GPa
386 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific)
Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating..
Flexural Modulus 2.66 GPa
386 ksi
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data)
Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos..
Flexural Modulus 2.66 GPa
386 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® BPL1000 PC
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Flexural Modulus 2.66 GPa
386 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Flexural Modulus 2.66 GPa
386 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Flexural Modulus 2.66 GPa
386 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Flexural Modulus 2.66 GPa
386 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Flexural Modulus 2.66 GPa
386 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS/PC FC-30
Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.66 GPa
386 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.66 GPa
386 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..