Flexural Modulus 1.24 - 2.76 GPa
180 - 400 ksi
Average value: 1.99 GPa Grade Count:18
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Modulus 2.07 - 2.76 GPa
300 - 400 ksi
ASTM D790
Alcoa KAMA 5100 CPET  (discontinued **)
CapabilitiesGauge: .020" to .040" (508 to 106µm)Width: 20" to 52" (508 to 1321mm)Core size: 3" or 6"Roll O.D.: 29" standard, available up to 40"Silicone coating availableAvailable in natural blackP..
Flexural Modulus 1.38 - 2.76 GPa
200 - 400 ksi
ASTM D790
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an..
Flexural Modulus 1.38 - 2.76 GPa
200 - 400 ksi
ASTM D790
Alcoa KAMA 3210 Hi-Gloss Coextruded High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat..
Flexural Modulus 1.37 - 2.76 GPa
199 - 400 ksi
Average value: 2.09 GPa Grade Count:36
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Flexural Modulus 2.07 - 2.76 GPa
300 - 400 ksi
Average value: 2.40 GPa Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Flexural Modulus 1.38 - 2.76 GPa
200 - 400 ksi
ASTM D790
Alcoa KAMA 3200 Prime High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea..