Polymer Property : Flexural Modulus = 2.76 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0190 GPa
2.76 ksi
ASTM D790
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where..
Flexural Modulus 0.0190 GPa
2.76 ksi
ASTM D790
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, ..
Flexural Modulus 0.0190 - 0.0960 GPa
2.76 - 13.9 ksi
Average value: 0.0561 GPa Grade Count:15
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Flexural Modulus 0.0190 GPa
2.76 ksi
1% Secant, ASTM D790
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile..
Flexural Modulus 0.0190 - 0.0372 GPa
2.76 - 5.40 ksi
Average value: 0.0274 GPa Grade Count:3
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..