Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.2 GPa @Temperature 149 °C |
2200 ksi @Temperature 300 °F |
ASTM D790 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | Tangent |
Premix Premi-Glas® 1200-50VE 1200-50 VE SMC
(discontinued **) Description: Premi-Glas® 1200-50 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-30GF-25MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-35GF-15MC/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 1020 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East) LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D 790 |
BCC Products Proto-Kast BC 8163 Urethane Casting BC 8163 is a very low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8163 is non-sensitive to moisture after cure and.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | Tangent; ASTM D790 |
Applied Composites 175 Vinylester SMC Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Flexural Modulus | 15.2 - 16.5 GPa | 2200 - 2400 ksi | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled