Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.42 GPa | 496 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific) LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010FV PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010RV PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1110FV PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.42 GPa | 496 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |