Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.53 GPa | 512 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505R PC Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505R PC (Europe-Africa-Middle East) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Kotec Carbotex KG-10MRA Polycarbonate, 10% Glass Fiber Reinforced Features: Glass fiber 10% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Kotec Carbotex KGN-10MRA Polycarbonate, Flame Retardant, 10% Glass Fiber Reinforced Features: Glass fiber 10% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Flexural Modulus | 3.53 GPa @Thickness 3.20 mm |
512 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1010 PC (Asia Pacific) |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Samyang Trirex® 3025G10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 3.53 GPa | 512 ksi | ASTM D790 |
Teknor Apex Sinpolene TPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 40% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Flexural Modulus | 3.53 GPa @Thickness 3.20 mm |
512 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |