Mechanical Properties Metric English Comments
Flexural Modulus 3.55 GPa
515 ksi
Tangent; ASTM D790
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 3.55 GPa
515 ksi
ASTM D790
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer
NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def..
Flexural Modulus 3.55 GPa
515 ksi
ASTM D790
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer
Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to..
Flexural Modulus 3.55 GPa
515 ksi
ISO 178
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C..
Flexural Modulus 3.55 GPa
515 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 4002 PEI
PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.
Flexural Modulus 3.55 GPa
515 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL HS2000X PPE+PS
PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E..
Flexural Modulus 3.55 GPa
515 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific)
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.
Flexural Modulus 3.55 GPa
515 ksi
1% secant; ASTM D790
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 3.55 GPa
515 ksi
1% secant; ASTM D790
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 3.55 GPa
515 ksi
1% secant; ASTM D790
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 3.55 GPa
515 ksi
1% secant; ASTM D790
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 3.55 GPa
515 ksi
1% secant; ASTM D790
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 3.55 GPa
515 ksi
1% secant; ASTM D790
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)
DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Modulus 3.55 GPa
515 ksi
ASTM D790, ISO 178
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber
Characteristics: 10% glass fibre filled, good mechanical properties
Flexural Modulus 3.55 GPa
515 ksi
ISO 178
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Flexural Modulus 3.55 GPa
515 ksi
Tangent; ASTM D790
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 3.55 GPa
515 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® X6320 PBT+PC
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP..