Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 3.75 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.75 GPa
544 ksi
ISO 178
Polycasa SAN
QUINN SAN sheets are characterized by good optical properties and a brilliant surface. The QUINN SAN range contains sheets that are easy to handle, to vacuum form, and show a very good dimensional s..
Flexural Modulus 3.75 GPa
544 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Flexural Modulus 3.75 GPa
544 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Flexural Modulus 3.75 GPa
544 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Flexural Modulus 3.75 GPa
544 ksi
ASTM D790
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific)
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.
Flexural Modulus 3.75 GPa
544 ksi
ISO 178
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Flexural Modulus 3.75 GPa
544 ksi
JIS-K-6740
Denka VINYKON R5020 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Flexural Modulus 3.75 GPa

@Temperature 93.0 °C
544 ksi

@Temperature 199 °F
ASTM Test
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Flexural Modulus 3.75 GPa
544 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1040 PP
SABIC® PPcompound 15T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound, suitable for injection molding applications. The IMDS ID is 16487994