Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific) Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM D790 |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Flexural Modulus | 2.27 GPa @Temperature 23.0 °C |
329 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp Noryl_SPN422L is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+PS LNP* Lubricomp* Noryl_SPN422L compound is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D2000P PC LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1390 PPE+PS Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2.0 mm/min, 3 point; ISO 178 |
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Resin Overview: CALIBREâ„¢ IM 401-18 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM D790 |
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer res.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM D790 |
Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux HS2 is produced from a FDA and USP Class VI approve.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | chs 2 mm/min; ASTM D790 |
Diamond Polymers DIAMALOY PC 1113 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | chs 2 mm/min; ASTM D790 |
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM Test |
BASF Ultramid® 8253 HS BK-102 PA6 (Dry) Ultramid 8253 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying leve.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC LNP LUBRICOMP* DL002 is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.27 GPa | 329 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EN185 PPE+PS Extrusion grade. Excellent impact strength. 185F (85C) DTUL. UL94 V-1 rated. |