Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.274 GPa | 329.8 ksi | ASTM D 790 |
MRC Polymers NAXELL™ PC210HR General Purpose Polycarbonate, High MFR • Black onlyInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.274 GPa @Thickness 3.17 mm |
329.8 ksi @Thickness 0.125 in |
tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABSPC 7030 ABS/PC Injection Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa @Thickness 6.35 mm |
329.8 ksi @Thickness 0.250 in |
tangent; chs 2.5 in/min; 100 mm SL; ASTM D790 |
Diamond Polymers ABSPC 7430-1005T ABS/PC Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 801 Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | ASTM D790 |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | ASTM D790 |
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers PC 0614UV UV Stabilized Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers PC 2418 R UV UV Stabilized/Mold Release Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.274 GPa | 329.8 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers PC-1514LUV UV Stabilized Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |