Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.72 - 3.10 GPa | 249 - 450 ksi | ASTM D790 |
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC) Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne |
|||
Flexural Modulus | 1.96 - 3.10 GPa | 284 - 450 ksi | Average value: 2.32 GPa Grade Count:33 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Modulus | 0.945 - 3.10 GPa | 137 - 450 ksi | Average value: 2.55 GPa Grade Count:25 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Flexural Modulus | 1.03 - 3.10 GPa | 149 - 450 ksi | Average value: 1.89 GPa Grade Count:27 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 0.965 - 3.10 GPa | 140 - 450 ksi | Average value: 1.67 GPa Grade Count:17 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |