Mechanical Properties Metric English Comments
Flexural Modulus 7.58 - 31.0 GPa
1100 - 4500 ksi
Average value: 17.3 GPa Grade Count:11
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Modulus 4.50 - 31.0 GPa
653 - 4500 ksi
Average value: 15.4 GPa Grade Count:50
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 11.7 - 31.0 GPa
1700 - 4500 ksi
Average value: 22.6 GPa Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Flexural Modulus 11.0 - 31.0 GPa
1600 - 4500 ksi
Average value: 26.6 GPa Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..