Mechanical Properties Metric English Comments
Flexural Modulus 14.8 - 33.1 GPa
2150 - 4800 ksi
Average value: 22.9 GPa Grade Count:12
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..