Mechanical Properties Metric English Comments
Flexural Modulus 14.8 GPa
2150 ksi
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre
FeaturesChemically reinforced with 40% carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. ..
Flexural Modulus 14.8 GPa
2150 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Flexural Modulus 14.8 GPa

@Temperature 150 °C
2150 ksi

@Temperature 302 °F
ASTM D790
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Modulus 14.8 GPa
2150 ksi
ISO 178
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
Flexural Modulus 14.8 GPa
2150 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Flexural Modulus 14.8 GPa
2150 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UF00AAS PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF00AAS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include: Heat Stabilized.
Flexural Modulus 14.8 GPa
2150 ksi
ISO 178-93
Wellman Wellamid® GF1750-BK2 50% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Flexural Modulus 14.8 GPa
2150 ksi
ASTM D790
Plenco 6401 Phenolic, Briquette, Injection Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Flexural Modulus 14.8 - 33.1 GPa
2150 - 4800 ksi
Average value: 22.9 GPa Grade Count:12
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Flexural Modulus 14.8 GPa
2150 ksi
ISO 178
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0...