Mechanical Properties Metric English Comments
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6821 BLK
This product is based on Kraton G and PP suitable for automotive applications and meets GM, Ford, and Chrysler specifications. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 7318 GREY
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 M BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 8002 BLK
Multi-Flex® TPE 8002 is based on Shell's Kraton G polymer technology and is widely used in the automotive industry for applications requiring elastomeric performance with excellent ozone resistance..
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 C BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 C GREY
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 C NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 E UV BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 HR BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6221 NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.0345 GPa
5.00 ksi
ASTM D790
Multibase Multi-Flex® A 6221 C TPE Thermoplastic Elastomer
Forms: PelletsInformation provided by Multibase