Polymer Property : Flexural Modulus = 5.70 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.44738 - 5.70 GPa

@Temperature 60.0 - 120 °C
500.008 - 827 ksi

@Temperature 140 - 248 °F
Average value: 4.45 GPa Grade Count:2
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Flexural Modulus 1.50 - 5.70 GPa
218 - 827 ksi
Average value: 3.21 GPa Grade Count:175
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..