Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.76 GPa | 835 ksi | 2mm/min; ASTM D790 |
Kingfa PA6-G15 15% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Modulus | 5.76 GPa | 835 ksi | ASTM Test |
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry) Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low.. |
|||
Flexural Modulus | 5.76 GPa | 835 ksi | ASTM Value |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |