Polymer Property : Flexural Modulus = 835 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.76 GPa
835 ksi
2mm/min; ASTM D790
Kingfa PA6-G15 15% Glass Fiber Reinforced PA6
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Flexural Modulus 5.76 GPa
835 ksi
ASTM Test
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry)
Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low..
Flexural Modulus 5.76 GPa
835 ksi
ASTM Value
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi..