Polymer Property : Flexural Modulus = 5.99 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.99 GPa
869 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied..
Flexural Modulus 5.99 GPa
869 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 (Asia Pacific)
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied..
Flexural Modulus 5.99 GPa
869 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY DF204 PC
LNP* LUBRILOY* DF204 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added feature of th is grade is: Wear Resistant.
Flexural Modulus 5.99 GPa
869 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS
LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s).
Flexural Modulus 5.99 GPa
869 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC
LNP THERMOCOMP* DF004P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing.
Flexural Modulus 5.99 GPa
869 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX06420 PA 66
LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release.
Flexural Modulus 5.99 GPa
869 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall.
Flexural Modulus 5.99 GPa
869 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS
LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall.
Flexural Modulus 5.99 GPa
869 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant..
Flexural Modulus 5.99 GPa
869 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific)
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.