LNP* Thermocomp* RX06420 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Low Extractible, Mold Release.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow >= 0.020 cm/cm

@Time 86400 sec
>= 0.020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Flexural Strength 161 MPa
23400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.58 GPa
809 ksi
2 mm/min; ISO 178
5.99 GPa
869 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.440 J/cm
0.824 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.98 J/cm
7.46 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 219 °C

@Thickness 3.20 mm
426 °F

@Thickness 0.126 in
unannealed; ASTM D648