Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | |
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790M-93 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Flexural Modulus | 3.60 - 8.90 GPa | 522 - 1290 ksi | Average value: 6.97 GPa Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2mm/min; ASTM D790 |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Flexural Modulus | 3.60 GPa @Thickness 3.20 mm |
522 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Higlass BJ22GC Polypropylene Copolymer, 30% Glass Fiber Key Features: conventional melt flow, medium high modulus, UV-stabilized, chemically coupled, glass fiber-reinforced polypropylene copolymer, moderately high rigidity, high impact strength, excellen.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ BC142/1AC Polypropylene Copolymer Description: Hostacomâ„¢ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It.. |
|||
Flexural Modulus | 3.60 GPa @Temperature 175 °C |
522 ksi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2mm/min; ISO 178 |
Teijin Panlite® G-3410R Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | Tangent; ASTM D790 |
Washington Penn PPUP4G402 Polypropylene, 40% Talc Filled, High Flow Exceptional retention of mechanical properties and appearance upon long term heat aging.Applications: Appliance parts.Data provided by Washington Penn Plastic Co., Inc. |
|||
Flexural Modulus | 3.60 GPa @Temperature 260 °C |
522 ksi @Temperature 500 °F |
ASTM D790 |
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM-D790 |
Polyram PlusTek PB340S6 Nylon 6, 30% Glass beads 30% glass beads reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM-D790 |
Polyram RamOfin PPC364I6 Polypropylene, 30% Mineral and Glass Fiber 30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D 790 |
Cossa Polimeri ESTABLEND 0820 GF Polycarbonate ABS Blend, 10% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 10% glass fiber reinforcementGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D 790 |
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polycarbonate POL051G10L Glass Reinforced |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334G10M20CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L1 Talc Reinforced |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polypropylene HP0335T40V Homopolymer Talc Reinforced Approved to ESF-M4D355B White B12391 |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Ashley Polymers Ashlene® 525-13G Nylon 66, 13% Glass Reinforced High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ISO 178 |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ISO 178 |
BASF Ultramid® C3U10 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Ashley Polymers Ashlene® P1410 Polycarbonate, 10% Glass Reinforced A 10% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1413: with UV stabilizer.Data provided by the manufacturer |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)