Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVASTER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVASTER® B1 GF 15 FRX 5 PBT reinforced with 15% glass fibre, with flame retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PBT with the content of 15 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other hole products. Application in engineering, electrical and automotive industry. High mechanical properties also in conditioned state. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 250 °C
10 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 5.20 GPa
754 ksi
Flexural Strength 90.0 MPa
13100 psi
Flexural Modulus 3.60 GPa
522 ksi
Charpy Impact Unnotched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
3.50 J/cm²

@Temperature -20.0 °C
16.7 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 0.180 J/cm²

@Temperature -20.0 °C
0.857 ft-lb/in²

@Temperature -4.00 °F
0.250 J/cm²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 200 - 220 °C
392 - 428 °F
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
Vicat Softening Point 205 °C
401 °F
Flammability Test 5.0

@Thickness 0.800 mm
5.0

@Thickness 0.0315 in
Glow Wire Test 960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in
Comparative Tracking Index 600 V
600 V
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 50.0 - 90.0 °C
122 - 194 °F
Drying Temperature 120 °C
248 °F
Dry Time 2 hour
2 hour
Moisture Content 0.050 %
0.050 %
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi