Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.373 - 9.00 GPa | 54.0 - 1310 ksi | Average value: 4.01 GPa Grade Count:61 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Flexural Modulus | 0.373 GPa @Thickness 3.20 mm |
54.0 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 0.372 GPa | 54.0 ksi | ASTM D790 |
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |