Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.15 GPa | 892 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific) CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla.. |
|||
Flexural Modulus | 6.15 GPa | 892 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
Flexural Modulus | 6.15 GPa | 892 ksi | |
Plastcom SLOVAMID 6 NG GF 20 HLS PA6, 20% glass fibre, combined stability FeaturesPA 6 for injection moulding, chemically reinforced with 20% glass fibre, heat stabilized and weather stabilized. Stabilized against hydrolysis. Good surface finisch.Packaging, transport, sto.. |
|||
Flexural Modulus | 6.15 GPa | 892 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Flexural Modulus | 6.15 GPa | 892 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS LNP* THERMOCOMP* AF004 is a compound based on ABS resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 6.15 GPa | 892 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Flexural Modulus | 6.15 GPa | 892 ksi | ISO 178 |
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |